对助焊剂的活性组分和其他组分采用正交试验进行筛选,根据工业标准对其进行了焊料铺展面积测试,效果较好的活性剂进行复合处理,对配制出的活性剂溶液加入松香配制成助焊剂进行性能测试.结果表明:当有机酸和三乙醇胺的质量比为12:1,占助焊剂质量分数的13.68%时,溶液的pH值达到3.94,扩展率可达80.06%,钎焊后的焊点光亮、无飞溅、残留量低.