收录:
摘要:
Barium calcium aluminate (4BaO:CaO:Al2O3) was synthesized via liquid phase co-precipitation and solid phase mixing respectively and sintered in hydrogen atmosphere. Scandia doped tungsten powders were prepared in a new process of spray drying combined with two-step hydrogen reduction. During the preparation of scandia doped impregnated cathodes, a series of procedures, including pressing, sintering, impregnating, water cleaning and annealing were taken to obtain the impregnated cathodes. The results show that Ba5CaAl4O12 is formed after high temperature sintering. After impregnation, scandia doped impregnated cathodes with porous sub-micron structure are obtained. For full activation at 1150 degrees C, the cathode surface is covered by a Ba-Sc-O active substance layer with a preferable atomic ratio, leading to its good emission property with space charge limited current density of 37.89 A/cm(2) at 850 degrees C.
关键词:
通讯作者信息: