The scandia doped tungsten powders have been obtained by a new method of spray drying combined with two-step reduction in hydrogen atmosphere. The impregnated cathode prepared with the obtained powders has an excellent emission capability of 121 A/cm(2) at 950 degrees C b in pulsed condition. The DC life test result indicates that the emission current density of 40 A/cm(2) has lasted up to 4000 hours.