一种渗碳La[2]O[3]和Lu[2]O[3]共掺杂Mo丝阴极,由La[2]O[3]和Lu[2]O[3]掺杂的钼(Mo)粉末制成, 氧化镧(La2O3)和氧化镥(Lu2O3)掺杂的钼(Mo)粉末含有La2O3,Lu2O3和Mo,La2O3和Lu2O3的总浓度为2.0-5.0wt%。 其余为钼。