A tri-layer composite ingot with Ni-5%W (mole fraction) alloy as the outer layer coupled with Ni-12%W (mole fraction)alloy as the inner layer was fabricated by sparking plasma sintering method. A 10 m length composite tape was prepared by traditional hot rolling and cold rolling process. The results show that the connectivity between the outer layer and inner layer of the composite tape is good enough during the heavy cold rolling process. The evaluation of the uniformity for both the thickness and texture in the whole tape shows that the thickness of the obtained composite tape is (75 ± 3)μm and the cube texture is about 97% (