By adding 1.5 mol.% Bi(Mn2/3Sb1/3)O-3 (BMS), (Bi1/2K1/2)TiO3 (BKT) ceramics show an excellent sintering ability in conventional oxide sintering process. In a wide temperature range from 1020-1050 degrees C, the 0.985BKT-0.015BMS (BKMS) ceramics demonstrate a super-high relative density of 98% and low dielectric loss tan delta of 0.017. Even though the temperature reaches to 1060 degrees C, BKMS ceramics maintain high relative density over 95% other than being collapsed as the pure BKT did. Besides, the BKMS ceramics sintered at 1020 to 1050 degrees C present adequately high electrical properties. The enhanced sintering ability of BKMS ceramics is attributed to the increased viscosity of liquid induced by Sb5+ solving in the liquid phase during sintering. The work provides a way to realize the densification of BKT ceramics. (C) 2019 The Ceramic Society of Japan. All rights reserved.
关键词:
通讯作者信息:
电子邮件地址:
来源 :
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN
ISSN: 1882-0743
年份: 2019
期: 4
卷: 127
页码: 215-220
1 . 1 0 0
JCR@2022
ESI学科: MATERIALS SCIENCE;
ESI高被引阀值:211
JCR分区:3