Due to the status quo of lack of data about high-tensile steel in H2S environment, the fatigue crack growth rate of 4130X steel used in compressed H2S vessel was investigated. Considering its practical operating ambient and stress condition, after overcoming enormous difficulties, the self-modified WOL(wedge-opening-loading) specimens were used in the specifically designed low-cycle corrosion fatigue testing machine, in order to complete the tests under 0.0067 Hz, in saturated H2S, moderate concentration and air environment, respectively. Moreover, the mathematical expression of da/dN-ΔK was concluded by the fitted curve using Paris formula. Contrast study between the changes of the specimens' microscopic fracture and the stress intensity factor K was conducted. Therefore, the quantitive result of K of three stages in different environment was determined. The results show that: 1) da/dN in H2S environment is above 20 times of that in air environment. 2) when the concentration of H2S reaches to a certain range, its effect on da/dN is not scaled up. da/dN differs by 2.4 times while the concentration differs by 11 times. The corrosion medium accelerates the fatigue failure.
关键词:
通讯作者信息:
电子邮件地址: